Researchers control where ultrathin semiconductor crystals form

Oxygen released by patterned oxide barriers suppresses growth near the edges, leaving the centre to start a single crystal in laboratory experiments.

Oxygen released by patterned oxide barriers suppresses growth near the edges, leaving the centre to start a single crystal in laboratory experiments.
Researchers report a way to make molybdenum disulfide (MoS2), a semiconductor grown here as a sheet one layer thick, begin forming crystals at the centre of patterned regions. Their study, published in Nature on 7 October, uses oxygen released from a surrounding oxide barrier to suppress crystal formation near the edges.
The method addresses a limitation of conventional area-selective growth, which deposits material in chosen regions while blocking it elsewhere. In the paper’s comparison, crystals can start at random locations throughout the allowed region. Shrinking that region can produce a single crystal, but does not fix its starting position. The authors identify this randomness as a constraint on crystal size and reliable placement.
The researchers surround exposed growth regions with hafnium oxide (HfO2). During deposition, the barrier releases oxygen that can etch away MoS2. In the authors’ model, oxygen concentration falls with distance from the barrier. Etching therefore suppresses nucleation—the formation of the first stable crystal seed—near the edges, while growth can exceed etching in a small central region. This makes the centre the most likely starting point.
For the main demonstration, the team grew MoS2 on patterned sapphire using metal–organic chemical vapour deposition, a process that supplies chemical ingredients as vapours. Scanning electron microscope images showed crystals starting at the centres and then spreading sideways to fill the regions. Electron diffraction, atomic-resolution microscopy and optical measurements also supported the finding that the flakes were single crystals: one continuous crystal structure rather than several joined grains.
The oxide-control experiments support oxygen’s role. Among the oxides compared under identical deposition conditions, only HfO2 suppressed MoS2 nucleation; oxygen released from that barrier could also completely etch away MoS2. At the usual process temperature of 750°C, X-ray photoelectron spectroscopy, which measures chemical composition, showed the barrier’s oxygen content falling from HfO1.95 to HfO1.83 within 10 minutes before levelling off. The authors interpret that change as evidence of oxygen release.
The barrier does not guarantee one crystal under every condition. At a fixed process time, a region can be too small for growth to overcome etching anywhere. An intermediate size can leave one central starting region, while a larger pattern can leave enough space for several seeds. The paper illustrates this with three growth-region sizes.
| Growth-region size | Observed crystal seeds |
|---|---|
| 3 micrometres | None |
| 5 micrometres | One |
| 7 micrometres | Several |
Time changes that balance. As processing continues, the authors report that oxygen release and etching decline, expanding the area where seeds can form and increasing nucleation. Larger regions begin nucleating earlier because their centres experience less etching. Maintaining a single starting point therefore depends on matching pattern size to the changing oxygen supply.
Deposition chemistry matters too. The paper reports no seeds, one seed or several seeds under different reaction conditions. The authors attribute their process’s greater sensitivity to oxygen-induced etching, compared with earlier MoS2 growth on HfO2, to the precursor type—the chemical feed used to grow the material.
The researchers report a single-crystal yield exceeding 99% across 400 patterned sites on a 2-cm substrate. The sites were arranged in 16 regions, each containing 25 patterns. This shows that the method worked repeatedly across the tested substrate, rather than only at an isolated site.
In a separate demonstration at 430°C, the team used a zirconium dioxide (ZrO2) barrier on silicon dioxide (SiO2) and reported uniformly centred, triangular single-crystal MoS2 domains. The authors chose ZrO2 because it has a lower crystallization temperature than HfO2. HfO2’s reduced oxygen release below 500°C may hinder the method. The greater-than-99% yield should not be read as the reported yield of this separate 430°C experiment.
The authors present these results as a route towards larger-area integration of ultrathin semiconductor crystals. The experiments establish laboratory control over where crystals start growing; they do not by themselves establish industrial production performance. Whether that control can be maintained under industrial manufacturing conditions remains an open question.

Blood and stool comparisons from more than 200 people add human context to the October 7 mouse findings, not proof of a treatment benefit.
3 min

An archival study examines how the industry challenged scientific evidence and advice to eat less meat in the late 1980s and early 1990s.

A structure from Methanosarcina acetivorans links enzyme inhibition to the cell's energy and nitrogen status.