MicroQuanta team reports 23.9% solar module efficiency


The team says its 19.48 cm² perovskite mini-module set a world record, using a cooling step intended to reduce losses as solar cells are combined into modules.
A research team led by MicroQuanta Semiconductor scientists achieved a steady-state conversion efficiency of 23.9% with a 19.48 cm² perovskite solar mini-module, pv magazine said on 19 November. The publication and corresponding author Dongchen Lan called the result a world record, although the sizes, area definitions and test conditions used for the comparison are not specified. Lan said the claimed record was achieved at module level rather than in a small laboratory cell.
In March 2025, Solarbe described an earlier MicroQuanta mini-module of the same area with a full-area steady-state efficiency of 23.93%. It said the National PV Industry Measurement and Testing Center had certified that result. Whether it was the device described in the later study is unclear.
Pv magazine said the center, part of the Fujian Metrology Institute, certified the later result. A certificate independently tying that result to the study’s device has not been identified.
Perovskite solar cells use a light-absorbing layer to generate electrical charge. The mini-module joined eight smaller cells in a series using laser scribing. Conversion efficiency measures electrical output against incoming light power; a higher figure means more of that light is converted to electricity.
Solar cells often lose efficiency when scaled up into modules.
The researchers compared laboratory cells with mini-modules made under matched conditions. After accounting for current losses in inactive areas created by laser scribing, they found that electrical fill factor was the largest contributor to the measured efficiency drop. Fill factor compares a device’s maximum power output with the product of its open-circuit voltage and short-circuit current.

The team said cooling the wet material before vacuum treatment slowed crystallization and reduced those losses. Its mini-module had an electrical fill factor of 83.3%. The source does not make clear whether the authors' highest-result claim refers to fill factor, efficiency or both. A separate measure, geometric fill factor, was 97%: that was the share of the module’s aperture area that responded to light.
Measurements during film formation showed that cooling slowed the conversion of an intermediate phase into perovskite, producing films with larger, more uniform grains. The separate aging test was a laboratory comparison, not a demonstration of commercial-panel durability.
In separate aging tests under continuous one-sun illumination at open circuit, the efficiency loss attributed to declining fill factor was less than one-third as large in modules made with cooling as in control modules. The study, published in Nature Communications, included researchers from Zhejiang University, China Three Gorges Renewable, the Zhejiang Provincial Key Laboratory of Optoelectronic Functional Materials and Devices, and the Australian Centre for Advanced Photovoltaics.
The wallet maker confirmed a few altered devices in Berlin. Separately, Bitquery estimates about $1.68 million was taken from 16 wallets linked to buyers’ reports in the two cities; Ledger is still examining the Dubai devices.
3 min

Quaise Energy says the agreement is worth more than $500 million. Google plans to use power from the Oregon project for its existing data centers as early as 2030.
2 min

Etsy’s new terms will permit superintelligence training on seller uploads from 16 December 2026. Artists are closing shops and directing customers elsewhere because they do not want their work used for training.
1 min